ASTM A213

This standard specification for seamless ferritic and austenitic alloy steel boiler, superheater and heat-exchanger tubes.

This standard includes many steel grades

 (Ferritic steel): Gr.T2, Gr.T5, Gr.T5b, Gr.T5c, Gr.T9, Gr.T11, Gr.T12, Gr.T17, Gr.T21, Gr.T22, Gr.T91, Gr.T92, 18Cr-2Mo

(Austenitic Steel): TP201, TP202, TP304, TP304H, TP304N, TP304LN, TP304L, TP309cb, TP309H, TP309S, TP310Cb, TP310H, TP310HCb, TP310HCbN, TP310S, TP316, TP316H, TP316L, TP316N, TP321, ……etc.

Chemical Composition:

Grade C % Mn % P % S % Si % Cr % Mo% V %
T2 0.10-0.20 0.30-0.61 ≤0.025 ≤0.025 0.10-0.30 0.50-0.81 0.44-0.65 —
T5 max:0.15 0.30-0.60 ≤0.025 ≤0.025 0max:0.50 4.00-6.00 0.45-0.65 —
T5b max:0.15 0.30-0.60 ≤0.025 ≤0.025 1.00-2.00 4.00-6.00 0.45-0.65 —
T5c max:0.12 0.30-0.60 ≤0.025 ≤0.025 max:0.50 4.00-6.00 0.45-0.65 —
T9 max:0.15 0.30-0.60 ≤0.025 ≤0.025 0.25-1.00 8.00-10.00 0.90-1.10 —
T11 0.05-0.15 0.30-0.60 ≤0.025 ≤0.025 0.50-1.00 1.00-1.50 0.44-0.65 —
T12 0.05-0.15 0.30-0.61 ≤0.025 ≤0.025 max:0.50 0.80-1.25 0.44-0.65 —
T17 0.15-0.25 0.30-0.61 ≤0.025 ≤0.025 0.15-0.35 0.80-1.25 — 0.15
T21 0.05-0.15 0.30-0.60 ≤0.025 ≤0.025 max:0.50 2.65-3.35 0.80-1.06 —
T22 0.05-0.15 0.30-0.60 ≤0.025 ≤0.025 max:0.50 1.90-2.60 0.87-1.13 —
T91 0.08-0.12 0.30-0.60 ≤0.025 ≤0.025 0.20-0.50 8.00-9.50 0.85-1.05 0.18-0.25
18Cr-2Mo max0.025 max:1.00 ≤0.040 ≤0.030 max:1.00 17.5-19.5 17.5-2.5 —

Mechanical Property:

Steel Grade TS (Mpa) Ys (Mpa) E (%) Hardness
T2  ≥ 415 ≥ 205 ≥ 30 163 HB / 85 HRB
T5  ≥ 415 ≥ 205 ≥ 30 163 HB / 85 HRB
T5b  ≥ 415 ≥ 205 ≥ 30 179 HB/89 HRB
T5c  ≥ 415 ≥ 205 ≥ 30 163 HB / 85 HRB
T9 ≥ 415 ≥ 205 ≥ 30 179 HB/89 HRB
T11 ≥415 ≥ 205 ≥ 30 163 HB / 85 HRB
T12 ≥415 ≥ 205 ≥ 30 163 HB / 85 HRB
T17 ≥415 ≥ 205 ≥ 30 163 HB / 85 HRB
T21 ≥415 ≥ 205 ≥ 30 163 HB / 85 HRB
T22 ≥415 ≥ 205 ≥ 30 163 HB / 85 HRB
T91 ≥585 ≥ 415 ≥ 20 250 HB/ 25 HRC
18Cr-2Mo ≥ 415 ≥275 ≥ 20 217 HB/ 96 HRB